PLYWOOD: Cara setting short core veneer di pabrik.

STUDI REPORT: SHORT CORE (SC) SETTING AT SPB2 BINTULU

At SPB Bintulu, especially at SPB1, setting of short core (SC) are:

Description of picture is:

All of strings face to the bellow. So if be sett with long core (LC) and Face Back, the result:

Strings not face Face veneer, but still face Back veneer. At putty process, some time Back veneer become Face, and Face veneer become back veneer because Back veneer beter than Face. This condition happened at SPB2 Bintulu, and quality of panel of TY4, especially bonding strength, will not be optimum.

short core setting

short core setting

This case, effected at inspection process. If I found the face veneer defectively, so can not  do change the back become face veneer, because string position if the back veneer become face veneer faced face veneer (not standard). So the conclusion, if found face veneer defect, become defect item (UTY or reject) directly, no alternative.

To reduce defect, I hope setting of SC will be change. This condition have been inform to millside (Supervisor of composer).

Best Regards,

Rudi Hermawan.

Perihal Rudi Hermawan
Ku dilahirkan di daerah terpencil, jauh dari keramaian. Beberapa puluh tahun kemudian baru tahu keramaian kota. Dan dari keadaan tersebut sedikit banyak mewarnai gaya tuturku dalam tulisan. Tapi, siapapun itu orangnya yang membuat tulisan, tidak terlalu perlu untuk diperhatikan, yang perlu diperhatikan adalah isi pesan dari tulisan itu. Semoga bermanfaat.. :)

Tinggalkan Balasan

Isikan data di bawah atau klik salah satu ikon untuk log in:

Logo WordPress.com

You are commenting using your WordPress.com account. Logout / Ubah )

Gambar Twitter

You are commenting using your Twitter account. Logout / Ubah )

Foto Facebook

You are commenting using your Facebook account. Logout / Ubah )

Foto Google+

You are commenting using your Google+ account. Logout / Ubah )

Connecting to %s

%d blogger menyukai ini: